A1 Vertaisarvioitu alkuperäisartikkeli tieteellisessä lehdessä

Epithelial cell attachment and adhesion protein expression on novel in sol TiO2 coated zirconia and titanium alloy surfaces




TekijätRiivari Sini, Närvä Elisa, Kangasniemi Ilkka, Willberg Jaana, Närhi Timo

KustantajaWILEY

Julkaisuvuosi2022

JournalJournal of Biomedical Materials Research Part B: Applied Biomaterials

Tietokannassa oleva lehden nimiJOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS

Lehden akronyymiJ BIOMED MATER RES B

Sivujen määrä9

ISSN1552-4973

eISSN1552-4981

DOIhttps://doi.org/10.1002/jbm.b.35111

Verkko-osoitehttps://onlinelibrary.wiley.com/doi/10.1002/jbm.b.35111

Rinnakkaistallenteen osoitehttps://research.utu.fi/converis/portal/detail/Publication/175727005


Tiivistelmä
An adequate mucosal attachment is important when it comes to preventing peri-implant inflammation. The aim of this study was to compare epithelial cell adhesion and adhesion protein expression on in sol TiO2-coated and non-coated zirconia and titanium alloy surfaces. Fifty-six zirconia and titanium discs were cut, and half of them were coated with bioactive TiO2-coating. To study the epithelial cell attachment, human gingival keratinocytes were cultivated on discs for 1, 3, 6, and 24 h. The cell proliferation was detected by cultivating cells for 1, 3, and 7 days. In addition, the levels of adhesion proteins laminin y2, integrin alpha 6, beta 4, vinculin, and paxillin were detected with Western Blot method. Furthermore, high-resolution imaging of the actin cytoskeleton and focal adhesion proteins was established. Longer-term cell culture (1-7 days) revealed higher cell numbers on the coated zirconia and titanium discs compared to non-coated discs. The difference was statistically significant (p < .05) after 24 h on coated zirconia and after 3 and 7 days on coated titanium discs compared to non-coated discs. Clear induction in the protein levels of laminin y2 and integrin alpha 6 were detected on both coated samples, meanwhile integrin beta 4 were clearly induced on coated titanium alloy. The microscope evaluation showed significantly increased cell spreading on the coated discs. According to this study, the in sol induced TiO2-coating increases keratinocyte attachment and the expression of adhesion proteins on coated zirconia and titanium in vitro. Consequently, the coating has potential to enhance the mucosal attachment on implant surfaces.