A1 Refereed original research article in a scientific journal

Degree of conversion and leached monomers of urethane dimethacrylate-hydroxypropyl methacrylate-based dental resin systems




AuthorsZhang M, Puska MA, Botelho MG, Sailynoja ES, Matinlinna JP

PublisherNIHON UNIV, SCHOOL DENTISTRY

Publication year2016

JournalJournal of Oral Science

Journal name in sourceJOURNAL OF ORAL SCIENCE

Journal acronymJ ORAL SCI

Volume58

Issue1

First page 15

Last page22

Number of pages8

ISSN1343-4934

DOIhttps://doi.org/10.2334/josnusd.58.15


Abstract

The degree of conversion (DC) and monomer leaching of three experimental urethane dimethacrylate (UEDMA)-hydroxypropyl methacrylate (HPMA)-based resin systems were studied. Three experimental resins (El: 70.6 wt% UEDMA + 27.4 wt% HPMA, E2: 80.6 wt% UEDMA + 17.4 wt% HPMA, E3: 90.6 wt% UEDMA + 7.4 wt% HPMA) and one control resin [C: 70.6 wt% bis-phenol A glycidyl methacrylate (bis-GMA) + 27.4 wt% methyl methacrylate (MMA)] were prepared. For the DC test, cylindrical specimens [1.5 mm (h) x 6 mm (d)] were scanned with an ATR-FTIR instrument before and after light-curing (n = 5). For the monomer leaching test, block-shaped specimens [5.67 mm (1) x 2.00 mm (w) x 2.00 mm (h)] were light-cured (n = 6), stored in a 75% ethanol:water solution for 3 days, and then analyzed with HPLC. The UEDMA-HPMA-based experimental groups showed higher DC (62-78%) than the bis-GMA-MMA-based control group (58-66%), and the DC decreased as the UEDMA content increased (P < 0.05). Amongst the four groups, E3 exhibited the lowest leaching of both mono methacrylate (0.1% HPMA) and dimethacrylate (<0.043% UEDMA) monomers after 30 or 40 s of curing. The UEDMA-HPMA-based resins, therefore, exhibited higher DC and less monomer leaching compared to the bis-GMA-MMA-based resin.